The Ф16 head chrome zirconium copper welding copper head welding electrode is part of the circuit of the spot welding machine. It conducts current and provides the heat source required for welding. The material of our company's welding electrode is chromium zirconium copper, which has good electrical and thermal conductivity, high hardness, wear resistance, explosion resistance, crack resistance, and softening resistance. The temperature is high, the electrode loss during welding is very small, and the welding speed is fast.
Specifications
|
Model No. |
T |
L |
Model No. |
T |
L |
|
MSC-1640-1 |
1/10 |
40 |
MSP-1640-1 |
1/10 |
40 |
|
MSC-1645-1 |
1/10 |
45 |
MSP-1645-1 |
1/10 |
45 |
|
MSC-1650-1 |
1/10 |
50 |
MSP-1650-1 |
1/10 |
50 |
|
MSC-1655-1 |
1/10 |
55 |
MSP-1655-1 |
1/10 |
55 |
|
MSC-1660-1 |
1/10 |
60 |
MSP-1660-1 |
1/10 |
60 |
|
MSC-1665-1 |
1/10 |
65 |
MSP-1665-1 |
1/10 |
65 |
|
MSC-1670-1 |
1/10 |
70 |
MSP-1670-1 |
1/10 |
70 |
|
|
|
|
|
|
|
|
MSC-1640-2 |
MT#2 |
40 |
MSP-1640-2 |
MT#2 |
40 |
|
MSC-1645-2 |
MT#2 |
45 |
MSP-1645-2 |
MT#2 |
45 |
|
MSC-1650-2 |
MT#2 |
50 |
MSP-1650-2 |
MT#2 |
50 |
|
MSC-1655-2 |
MT#2 |
55 |
MSP-1655-2 |
MT#2 |
55 |
|
MSC-1660-2 |
MT#2 |
60 |
MSP-1660-2 |
MT#2 |
60 |
|
MSC-1665-2 |
MT#2 |
65 |
MSP-1665-2 |
MT#2 |
65 |
|
MSC-1670-2 |
MT#2 |
70 |
MSP-1670-2 |
MT#2 |
70 |
|
Model No. |
T |
L |
Model No. |
T |
L |
|
MSF-1640-1 |
1/10 |
40 |
MSE-1640-1 |
1/10 |
40 |
|
MSF-1645-1 |
1/10 |
45 |
MSE-1645-1 |
1/10 |
45 |
|
MSF-1650-1 |
1/10 |
50 |
MSE-1650-1 |
1/10 |
50 |
|
MSF-1655-1 |
1/10 |
55 |
MSE-1655-1 |
1/10 |
55 |
|
MSF-1660-1 |
1/10 |
60 |
MSE-1660-1 |
1/10 |
60 |
|
MSF-1665-1 |
1/10 |
65 |
MSE-1665-1 |
1/10 |
65 |
|
MSF-1670-1 |
1/10 |
70 |
MSE-1670-1 |
1/10 |
70 |
|
|
|
|
|
|
|
|
MSF-1640-2 |
MT#2 |
40 |
MSE-1640-2 |
MT#2 |
40 |
|
MSF-1645-2 |
MT#2 |
45 |
MSE-1645-2 |
MT#2 |
45 |
|
MSF-1650-2 |
MT#2 |
50 |
MSE-1650-2 |
MT#2 |
50 |
|
MSF-1655-2 |
MT#2 |
55 |
MSE-1655-2 |
MT#2 |
55 |
|
MSF-1660-2 |
MT#2 |
60 |
MSE-1660-2 |
MT#2 |
60 |
|
MSF-1665-2 |
MT#2 |
65 |
MSE-1665-2 |
MT#2 |
65 |
|
MSF-1670-2 |
MT#2 |
70 |
MSE-1670-2 |
MT#2 |
70 |
Product Description
KEEP IN TOUCH
Picture a mild steel bracket that cracks at the weld after a few months of vibration. The material looks correct, the rod was forgotten in a damp drawer, and the welder ran a long arc at 160 A. The f...
READ MORE
Your new MIG unit runs well for the first hour. Then the arc begins to sag, spatter builds up, and the machine trips out. You replace the contact tip, check the gas, and clean the liner, but the prob...
READ MOREYou are rewiring a production cell to join steel rods before drawing or straightening. The two candidate machines on the quote are a flash butt welding machine and a regular butt welding machine. Bot...
READ MORE
Oxygen Hose Color: The Direct Answer Walk onto any welding floor in the U.S. and you will see a green hose connected to an oxygen regulator. In Europe, the same gas hose is blue. Both are correct und...
READ MORE
Your sheet metal line is producing inconsistent welds. It may not be the operator's technique. More often, the machine was never matched to the actual job. Before replacing anything, it helps to star...
READ MORE
Why Pipe Cutting Automation Is a Production Decision, Not Just a Tool Purchase In shops that fabricate pipe or tube, the cutting stage is where schedules are lost. An operator measures a length, mark...
READ MORE